The invention discloses a making method of ice-crystal glaze, which comprises the following steps: adopting zinc oxide, lithium carbonate, titanium oxide, calcite, transparent fused block, kaolin, quartz flour and copper oxide as raw material with copper oxide as coloring oxide; balling through wet method; sieving; allocating slurry with density at 45-65 Baume's degree; fetching smooth ceramic blank to immerse glaze in the kiln; sintering in the oxidizing atmosphere under 1160-1200 deg.c rapidly; obtaining the product with glitter surface. |